Vickers Hardness to Rockwell Conversion Chart (FREE Downloadable Chart)

Vickers Hardness to Rockwell Conversion Chart (FREE Downloadable Chart)

·

If you’ve ever compared material specs across different reports, you’ve likely seen the need to convert Vickers hardness to Rockwell. Each scale reflects hardness in a slightly different way, yet they both help evaluate material strength, durability, and wear resistance. Converting between them isn’t always intuitive, but it’s manageable with the right tools and understanding.

In this article, we’ll walk you through why these conversions matter, how to use them correctly, and when to avoid assumptions that could cost your project accuracy.

Why Convert Vickers to Rockwell Hardness?

Hardness testing is a core method in quality control, especially for metals and alloys. Engineers, suppliers, and auditors often encounter results in Vickers (HV), while product specifications or standards require Rockwell (HRB or HRC).

Here’s why conversions are frequently needed:

  1. Supplier certificates use a different scale than in-house testing.
  2. Industry standards specify Rockwell C, but labs may report in Vickers.
  3. Comparative testing across international partners using ISO or ASTM methods.

Since Vickers and Rockwell use different indenters and loads, converting is not about applying a formula—it’s about referencing trusted conversion charts or standards like ASTM E140 (and its successors) or ISO 18265.

Understanding the Differences

Let’s quickly summarize the key differences between these two common hardness tests (and why direct conversion is never “one formula fits all”):

Vickers Hardness (HV)

  • Uses a diamond-shaped pyramid indenter.
  • Applied load is consistent, usually 1–100 kgf.
  • The indentation diagonal is optically measured under a microscope.
  • Excellent for microhardness or thin sections due to minimal surface damage.

Rockwell Hardness (HR)

  • Uses a steel ball or conical diamond depending on the scale.
  • Measures the depth of indentation under a specific load.
  • Fast and easy to automate—ideal for production environments.
  • Multiple scales: HRB (softer materials) and HRC (harder materials) are most common.

Since the measurement principles differ, Vickers to Rockwell conversion varies depending on material type, treatment, and test parameters. For a deeper comparison, read our full guide on the Vickers vs Rockwell hardness test.

Which Rockwell Scale Should You Convert To?

Rockwell ScaleIndenter & LoadTypical Use
HRB1/16″ ball, 100 kgfSofter metals (Al, Cu, brass), annealed steels, sheet goods
HRCDiamond cone, 150 kgfHardened steels, tool steels, heat-treated parts

Vickers to Rockwell B (HRB): Softer Metals Like Aluminum, Copper, and Brass

If you’re testing softer materials like aluminum alloys or annealed brass, you’re likely using Rockwell B scale. This scale uses a 1/16″ steel ball with a 100 kgf load.

Let’s look at a few sample conversions from the Qualitest chart:

Vickers to Rockwell B Hardness

You can see the relationship is non-linear, especially around the lower ranges. Always use a table rather than trying to calculate a value.

You can also download the Vickers to Rockwell B conversion table in PDF format here.

Vickers to Rockwell C (HRC): Hardened Steel and High-Strength Alloys

For hardened materials, tool steels, or heat-treated components, Rockwell C (HRC) is the go-to scale. It uses a diamond cone with a 150 kgf load and is more appropriate for surface-hardened or tempered components.

Here’s a snapshot from the second chart:

Vickers to Rockwell C Hardness

Conversion from Vickers to Rockwell C is often needed in tool manufacturing, aerospace, and automotive parts. However, even small errors can lead to misclassification of hardness grade.

The Vickers to Rockwell C conversion table is available in PDF format — download it here.

Factors That Influence Conversion Accuracy

Even when using official tables, there’s a margin of uncertainty. Several variables affect how reliable your conversion is:

  1. Material composition (steel vs. copper vs. titanium)
  2. Grain size or microstructure (e.g., cast vs. wrought)
  3. Heat treatment or work hardening
  4. Thickness and support/anvil conditions
  5. Surface preparation before testing (roughness, coatings, curvature)

Because of this, standards like ASTM E140 recommend that conversions be used only when direct measurement isn’t possible. If you’re testing on the go, understanding the accuracy of portable hardness testers can help you make more informed decisions when conversions are necessary.

Best Practices for Using Conversion Charts

When you’re working with Rockwell hardness to Vickers conversions or vice versa, follow these steps:

  1. Identify the correct Rockwell scale (e.g., HRB or HRC).
  2. Use verified conversion charts, such as those from ASTM or trusted manufacturers like Qualitest.
  3. Avoid converting values across drastically different material types (ferrous ↔ non-ferrous) without validation.
  4. Whenever feasible, test directly on the required scale instead of converting—it’s always more accurate.
  5. For documentation or reporting, label converted values as “approximate.”

Field Tip: Portable Testing & Conversions

  • Take multiple indents and average the result—then convert.
  • Match load/scale to thickness: micro-Vickers for case layers; HRC for through-hardened steels.
  • Record surface finish, load, dwell time, and indenter type alongside the converted value for full traceability.

Quick Workflow: From HV to the Right HR Scale

  1. Confirm material & condition (alloy family, heat treatment, thickness).
  2. Pick the Rockwell scale that matches the property range (HRB for softer; HRC for hardened steels).
  3. Use the correct table (ASTM E140 / ISO 18265 or the provided charts) within the applicable range.
  4. Document uncertainty and keep raw HV values alongside HR results.

Key Takeaways

  • Vickers and Rockwell measure hardness differently; conversions are empirical, not formulaic.
  • Always rely on official, material-appropriate tables (e.g., ASTM E140, ISO 18265).
  • Environment, surface prep, thickness, and microstructure affect both the base test and the conversion.
  • Where possible, test directly on the required scale to avoid reliance on conversions.

FAQ

1. What is the difference between Vickers and Rockwell hardness testing methods?

The Vickers test uses a diamond pyramid and measures the indentation diagonals (optical method), while Rockwell uses either a diamond cone or steel ball and measures indentation depth under load.


2. Why is it necessary to convert between Vickers and Rockwell hardness scales?

Different customers, specs, and regions require different scales. Conversion supports compliance, cross-industry comparison, and unified documentation.


3. What factors affect the accuracy of Vickers→Rockwell conversion?

Material composition, hardness range, heat treatment, thickness, surface condition, and the specific table used.


4. Can I use a conversion table for any material?

No. Use tables that apply to your material class and hardness range. Steel/iron alloys differ from aluminum, copper, titanium, etc.


5. How do I choose the correct Rockwell scale?

HRB for softer metals and annealed steels; HRC for hardened steels and high-strength alloys. See spec requirements.


6. Are there industry-specific applications where conversion is crucial?

Yes—automotive, aerospace, and general manufacturing often convert between HV and HR for receiving inspection and certification.


7. Common mistakes and how to avoid them?

Misreading tables, extrapolating outside valid ranges, and ignoring material specifics. Use updated standards, validated charts, and note uncertainty.


Further Reading

Related Products